1. It cannot be peeled off after being attached to the tape. Generally, it is the cause of uneven coating. Some of the release films have serious leakage, which will make a certain part have no release effect, so that the tape cannot be peeled off. The die-cutting of the circular knife should be I hate this question.
2. The greasy release surface is mainly caused by the release agent system. Not greasy things must be bad. In fact, some greasy release films are coated evenly on the surface and have better residual adhesion. But some are purely because of poor adhesion, and silicone oil is easy to fall off. These can also be determined by testing.
3. For static electricity problems, in addition to physical treatment methods, chemical treatment is permanent. Generally, photoelectric die-cutting factories have dust-free workshops and equipment for eliminating static electricity, so the problem will not be very big. . If the requirements are more stringent, the release film with antistatic coating can be selected.
4. There is a sound when peeling off, one is that the release force is too large, and the other is the result of uneven coating. There are many methods for judging whether the coating is uneven. One of the simpler ones is to look at the surface of the film against the light in the sun, and the surface coating effect of the film can be seen at a glance.
5. The anti-peeling is mainly caused by the unsatisfactory combination of the release force. There are two reasons. First, the release film is not strictly inspected at the factory, the inspection equipment is incomplete, and the production process is not stable enough, which makes the release force of the same type of product. Too much difference. As a result, the die-cutting factory used the release film with the release force they thought out of the habit. Second, the weather resistance of the release layer is not enough, and great changes have taken place over time.